296 Journal of Ceramic Science and Technology —A.E. Hannora Vol. 5, No. 4 Fig.5: XRD patterns of hydroxyapatite/alumina after sintering at 1200°C for three hours. Fig.6: TEM images with 15wt% alumina addition after sintering at 1200°C for three hours and electron diffraction pattern of an ordered phase. The mechanical properties are governed not only by